Polymer Property : CTE, linear, Parallel to Flow = 49.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.