Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 49.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38U ABS
High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG38U ABS
High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS
LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS
LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..