Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 35.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature 100 - 200 °C
19.4 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI
LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding.
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific)
LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature 100 - 200 °C
19.4 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific)
LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0049P PC
LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct..
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Copyright © lookpolymers.com All Rights Reserved