Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008S PP LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008S PP LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 46.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |