SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Xenoy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xenoy iQ4840 offers a good balance of impact and ductility, excellent pull strength, good fatigue, provides Class A surface which is paintable, and excellent processibilty. It is currently used in painted automotive doorhandles.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.0800 %
0.0800 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.28 %
0.28 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Melt Index of Compound 13 g/10 min

@Load 5.00 kg,
Temperature 265 °C
13 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.0 MPa
7830 psi
5 mm/min; ISO 527
60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa
8410 psi
5 mm/min; ISO 527
59.0 MPa
8560 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 120 %
120 %
5 mm/min; ISO 527
130 %
130 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.8 %
3.8 %
5 mm/min; ISO 527
3.9 %
3.9 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.80 GPa
551 ksi
1 mm/min; ISO 527
4.00 GPa
580 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 96.0 MPa
13900 psi
2 mm/min; ISO 178
104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
2 mm/min; ISO 178
3.50 GPa
508 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1A
8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
46.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 127 °C
261 °F
Rate B/50; ASTM D1525
128 °C
262 °F
Rate B/50; ISO 306
128 °C
262 °F
Rate B/120; ISO 306