CTE, linear, Parallel to Flow 43.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12
LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 43.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12
LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 43.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12
LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..