Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
12.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
12.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
12.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |