Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 32.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10 LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 32.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific) LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 32.2 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 32.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |