Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553 PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553 PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific)
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 553U PBT+PC
30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51 PBT
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51 PBT
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific)
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific)
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature -40.0 - 95.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..