Polymer Property : Hot Ball Pressure Test = 275 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics Lexan® 915R PC (Europe-Africa-Middle East)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
Hot Ball Pressure Test 135 °C
275 °F
Average value: 135 °C Grade Count:3
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Hot Ball Pressure Test 135 - 140 °C
275 - 284 °F
Average value: 137 °C Grade Count:6
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Hot Ball Pressure Test >= 135 °C
>= 275 °F
IEC 60335-1
Styron EMERGEâ„¢ 8702 Polycarbonate
EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Hot Ball Pressure Test <= 135 °C
<= 275 °F
IEC 60695-10-2
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East)
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 0400 OPALE Polycarbonate
Polycarbonate for injection or extrusionOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l.
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled
Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l.
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 0820 GF V0 HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good processability, good light resistanceI..
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation..
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g..
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 1060 V0 HF Flame Retardant Polycarbonate
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro..
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate
Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 1560 V0 HF Flame Retardant Polycarbonate
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro..
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 1601 OPALE Polycarbonate
Polycarbonate for injection moldingOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l.
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 1601 Polycarbonate
General purpose polycarbonateHigh melt flow rate, high impact resistanceInformation provided by Cossa Polimeri S.r.l.
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Cossa Polimeri ESTACARB 2060 V0 HF Flame Retardant Polycarbonate
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® 2667 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
Hot Ball Pressure Test 135 °C
275 °F
IEC 60695-10-2
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..