Polymer Property : Hot Ball Pressure Test = 248 °F
Polymer Property :
Hot Ball Pressure Test =
248 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Hot Ball Pressure Test
>=
120
°C
>=
248
°F
BS 3456, IEC 335
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber
Characteristics: 20% glass fibre filled