Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 795 °C | 1460 °F | |
Johnson Matthey Copper-flo AWS Alloy for Fluxless Brazing of Copper The copper-flo alloys are used for manufacture of heat exchanger return bends, refrigeration pipes and hot water cylinders.Optimum Joint Gap 0.75 - 0.2 mm.AWS A5.8-92 BCuP-2BS EN 1044 1999 CP202; Do.. |
|||
Liquidus | 795 °C | 1460 °F | |
Williams Advanced Alloys Wambraze™ WB795 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |