Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 795 °C | 1460 °F | |
Johnson Matthey Copper-flo AWS Alloy for Fluxless Brazing of Copper The copper-flo alloys are used for manufacture of heat exchanger return bends, refrigeration pipes and hot water cylinders.Optimum Joint Gap 0.75 - 0.2 mm.AWS A5.8-92 BCuP-2BS EN 1044 1999 CP202; Do.. |
|||
Liquidus | 793 °C | 1460 °F | Flow Point |
Lucas-Milhaupt FOS FLO 7 Copper Phosphorus Alloy Applications:Fos-Flo 7 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service.. |
|||
Liquidus | 793 °C | 1460 °F | |
Lucas-Milhaupt Silvaloy® 0 Brazing Alloy Silvaloy 0 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Liquidus | 795 °C | 1460 °F | |
Williams Advanced Alloys Wambraze™ WB795 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |