Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 310 °C | 590 °F | |
Nihon Superior SN100C3 High Temperature Dipper and Tinning Solder High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C. |
|||
Liquidus | 310 °C | 590 °F | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Liquidus | 310 °C | 590 °F | |
Indium Corp. Indalloy 12 Lead Solder Alloy Tin-free indium solderInformation Provided by Indium Corporation |
|||
Liquidus | 310 °C | 590 °F | |
Williams Advanced Alloys WS310 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |