Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atmospheres.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 11.02 g/cc
0.3981 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.4 MPa
4550 psi
Shear Strength 19.5 MPa
2830 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 300 - 310 °C
572 - 590 °F
Solidus 300 °C
572 °F
Liquidus 310 °C
590 °F
Component Elements Properties Metric English Comments
Indium, In 5.0 %
5.0 %
Lead, Pb 92.5 %
92.5 %
Silver, Ag 2.5 %
2.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000310 ohm-cm
0.0000310 ohm-cm
Copyright © lookpolymers.com All Rights Reserved