Thermal Properties Metric English Comments
Liquidus 302 °C
576 °F
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Liquidus 302 °C
576 °F
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy
High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation.
Liquidus 302 °C
576 °F
Williams Advanced Alloys WS302 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys