Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 10.75 g/cc
0.3884 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 10
10
Tensile Strength, Ultimate 30.3 MPa
4390 psi
Elongation at Break 30 %
30 %
Modulus of Elasticity 19.0 GPa
2760 ksi
Shear Strength 16.5 MPa
2390 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature 20.0 °C
16.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 275 - 302 °C
527 - 576 °F
Solidus 275 °C
527 °F
Liquidus 302 °C
576 °F
Component Elements Properties Metric English Comments
Lead, Pb 90 %
90 %
Tin, Sn 10 %
10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000190 ohm-cm
0.0000190 ohm-cm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved