Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 275 °C | 527 °F | |
Indium Corp. Indalloy® 150 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Liquidus | 275 °C | 527 °F | |
Johnson Matthey LM10A Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |