Material Notes:
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 10.27 g/cc
0.3710 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.3 MPa
5550 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K

@Temperature 85.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 260 - 275 °C
500 - 527 °F
Solidus 260 °C
500 °F
Liquidus 275 °C
527 °F
Component Elements Properties Metric English Comments
Indium, In 19 %
19 %
Lead, Pb 81 %
81 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000380 ohm-cm
0.0000380 ohm-cm