Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 226 °C | 439 °F | |
Indium Corp. Indalloy 123 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 226 °C | 439 °F | |
Indium Corp. Indalloy 260 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 226 °C | 439 °F | |
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Liquidus | 226 °C | 439 °F | |
Williams Advanced Alloys WS226A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |