Polymer Property : Liquidus = 226 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 226 °C
439 °F
Indium Corp. Indalloy 123 Tin Solder Alloy
Information Provided by Indium Corporation
Liquidus 226 °C
439 °F
Indium Corp. Indalloy 260 Tin Solder Alloy
Information Provided by Indium Corporation
Liquidus 226 °C
439 °F
Williams Advanced Alloys WS226 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Liquidus 226 °C
439 °F
Williams Advanced Alloys WS226A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys