Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 213 °C | 415 °F | |
Nihon Superior LF-C2 Lead-Free Solder Alloy |
|||
Liquidus | 213 °C | 415 °F | |
Indium Corp. Indalloy 118 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 213 °C | 415 °F | |
Indium Corp. Indalloy® 249 91.8Sn/3.4Ag/4.8Bi Lead-Free Solder Alloy Board & component metallizations must be Pb-free. U.S. Patent 5,439,639 (ICA Licensed Sandia Patent)Information provided by the manufacturer, Indium Corporation. |
|||
Liquidus | 213 °C | 415 °F | |
Williams Advanced Alloys WS213 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |