Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nihon Superior LF-C2 Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Nihon Superior
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nihon Superior LF-C2 Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Properties Metric English Comments
Melting Point 208 - 213 °C
406 - 415 °F
Solidus 208 °C
406 °F
Liquidus 213 °C
415 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 3.0 %
3.0 %
Copper, Cu 1.0 %
1.0 %
Silver, Ag 3.5 %
3.5 %
Tin, Sn 92.5 %
92.5 %
As Remainder
Users viewing this material also viewed the following: