Polymer Property : Liquidus = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 140 °C
284 °F
Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy
The addition of Ag adds mechanical strength. Good thermal fatigue performance; established history.Information provided by the manufacturer, Indium Corporation.