Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of Ag adds mechanical strength. Good thermal fatigue performance; established history.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.57 g/cc
0.310 lb/in³
Thermal Properties Metric English Comments
Melting Point 139 - 140 °C
282 - 284 °F
Solidus 139 °C
282 °F
Liquidus 140 °C
284 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 57 %
57 %
Silver, Ag 1.0 %
1.0 %
Tin, Sn 42 %
42 %