Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1010 °C | 1850 °F | |
Osprey Metals HTN 8 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Liquidus | 1010 °C | 1850 °F | |
Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy Applications: glass industry plungers and mold componentsInformation provided by Weartech International |
|||
Liquidus | 1010 °C | 1850 °F | |
Williams Advanced Alloys Wambraze™ WB1010 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |