Polymer Property : Liquidus = 1010 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1010 °C
1850 °F
Osprey Metals HTN 8 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Liquidus 1010 °C
1850 °F
Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy
Applications: glass industry plungers and mold componentsInformation provided by Weartech International
Liquidus 1010 °C
1850 °F
Williams Advanced Alloys Wambraze™ WB1010 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..