Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 79.0 °C | 174 °F | |
Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |