Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 173 °C | 343 °F | |
Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 173 °C | 343 °F | |
Indium Corp. Indalloy 240 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |