Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 816 °C | 1500 °F | |
Johnson Matthey Matti-sil 18Si Cadmium Free Brazing Alloy Matti-sil 18Si was developed as an economic alternative to the high silver alloys, particularly for steel automotive components where the higher temperature bronze alloys cannot be tolerated.Optimum.. |
|||
Liquidus | 816 °C | 1500 °F | |
Lucas-Milhaupt Silvaloy® A20 Brazing Alloy Silvaloy A20 can be used in a wide variety of applications but is infrequently used because of its relatively high melting point. It is an excellent choice when simultaneously brazing and heat treat.. |
|||
Liquidus | 814 °C | 1500 °F | |
Williams Advanced Alloys Wambraze™ WB814 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Liquidus | 815 °C | 1500 °F | |
Johnson Matthey Matti-phos 5 Alloy for Fluxless Brazing of Copper This alloy offer a good combination of flow and ductility. Like Matti-phos 6 it is used in air conditioning, refrigeration, medical gas pipework and heat exchanger manufacture.Optimum Joint Gap 0.0.. |