Johnson Matthey Matti-sil 18Si Cadmium Free Brazing Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Matti-sil 18Si Cadmium Free Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Matti-sil 18Si was developed as an economic alternative to the high silver alloys, particularly for steel automotive components where the higher temperature bronze alloys cannot be tolerated.Optimum Joint Gap 0.075 - 0.2 mm.Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 784 - 816 °C
1440 - 1500 °F
Solidus 784 °C
1440 °F
Liquidus 816 °C
1500 °F
Component Elements Properties Metric English Comments
Copper, Cu 45.75 %
45.75 %
Silicon, Si 0.25 %
0.25 %
Silver, Ag 18 %
18 %
Zinc, Zn 36 %
36 %