Polymer Property : Liquidus = 1410 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 766 °C
1410 °F
Flow Point
Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 300 is an intermediate temperature silver brazing alloy with a fairly long (160EF/70EC) melting range. This long melting range is helpful when wide gap joints are brazed and ..
Liquidus 766 °C
1410 °F
Lucas-Milhaupt Silvaloy® A30 Brazing Alloy
Silvaloy A30 does not contain cadmium and is often used as an alternate to cadmium containing alloys when the brazed assembly comes in contact with food or dairy products. Its slightly higher melt t..
Liquidus 765 °C
1410 °F
Johnson Matthey Matti-sil 30 Cadmium Free Brazing Alloy
The wide melting range of Matti-sil 30 makes it suitable for filling larger joint gaps and producing fillets where desired.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-20Federal Specification QQ..