Polymer Property : Liquidus = 1184 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 640.0 °C
1184 °F
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..