Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 105 °C | 221 °F | |
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 105 °C | 221 °F | |
Indium Corp. Indalloy 48 Bismuth Solder Alloy Information Provided by Indium Corporation |