Polymer Property : Solidus = 982 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 982 °C
1800 °F
approximate
Schmolz + Bickenbach MoldMAX® V Copper Alloy
Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores ..
Solidus 982 °C
1800 °F
Universal Wire Works BNi-4 (AMS 4779) Nickel Base Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.