Polymer Property : Solidus = 950 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 950 °C
1740 °F
Indium Corp. Indalloy 196 Gold Solder Alloy
Information Provided by Indium Corporation