Polymer Property : Solidus = 58.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 58.0 °C
136 °F
Indium Corp. Indalloy 21 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 58.0 °C
136 °F
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy
General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation.