Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 58.0 °C | 136 °F | |
Indium Corp. Indalloy 21 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 58.0 °C | 136 °F | |
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation. |