Polymer Property : Solidus = 513 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 267 °C
513 °F
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy
(Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation.