Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 267 °C | 513 °F | |
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy (Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation. |