Solidus 139 °C
282 °F
Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy
The addition of Ag adds mechanical strength. Good thermal fatigue performance; established history.Information provided by the manufacturer, Indium Corporation.