Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 138 °C | 280 °F | |
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m.. |
|||
Solidus | 138 °C | 280 °F | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 138 °C | 280 °F | |
AIM 40Bi/60Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Solidus | 138 °C | 280 °F | |
AIM 54Sn/26Pb/20In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Solidus | 138 °C | 280 °F | |
AIM 58Bi/42Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |