Thermal Properties Metric English Comments
Solidus 1302 °C
2375 °F
Carlson C 601 Nickel-Chromium-Iron Alloy
General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxida..