Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 960 °C | 1760 °F | |
Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing D Bronze is primarily used for the production of rock drills. Or where simultaneous heat treatment of the steel shank is required. Information provided by Johnson Matthey. |
|||
Solidus | 960 °C | 1760 °F | Melting Point |
Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing. Due to the high flow point of this alloy, torch brazi.. |
|||
Solidus | 960 °C | 1760 °F | Melting Point |
Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. We.. |
|||
Solidus | 960 °C | 1760 °F | |
Wieland 1703 Wilaform Gold Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental |
|||
Solidus | 961 °C | 1760 °F | |
Indium Corp. Indalloy 207 Pure Silver Information Provided by Indium Corporation |