Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 920 °C | 1690 °F | |
Wieland 1407 Wilaform Gold Red gold for all kinds of decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Solidus | 920 °C | 1690 °F | |
Wieland 1601 Wilaform Gold Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, .. |