Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1360 °C | 2480 °F | |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Solidus | 1360 °C | 2480 °F | |
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |