Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Solidus = 1325 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1325 °C
2417 °F
HP Alloys Alloy C-276, 10% Cold Worked
10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Solidus 1325 °C
2417 °F
HP Alloys Alloy C-276, 20% Cold Worked
20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Solidus 1325 °C
2417 °F
HP Alloys Alloy C-276, 40% Cold Worked
40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Solidus 1325 °C
2417 °F
HP Alloys Alloy C-276, 50% Cold Worked
50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® Alloy C-276
A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially ..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Bar
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special ..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Plate
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Sheet
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Solidus 1325 °C
2417 °F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Solidus 1325 °C
2417 °F
HP Alloys Alloy C-276, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Copyright © lookpolymers.com All Rights Reserved