Polymer Property : Solidus = 117 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 47.0 °C
117 °F
Indium Corp. Indalloy 16 Low Melting Bismuth Alloy
Information Provided by Indium Corporation
Solidus 47.0 °C
117 °F
Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.