Material Notes:
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 9.16 g/cc
0.331 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 16.5

@Load 4.00 kg
16.5

@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 37.2 MPa
5400 psi
Elongation at Break 37.5 %
37.5 %
% elongation on 5.65 (sq. root Area) gauge length
Thermal Properties Metric English Comments
Heat of Fusion 36.8 J/g
15.8 BTU/lb
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.163 J/g-°C
0.0390 BTU/lb-°F
Solid
0.197 J/g-°C
0.0471 BTU/lb-°F
Liquid
Thermal Conductivity 15.0 W/m-K

@Temperature 85.0 °C
104 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 47.0 °C
117 °F
Eutectic
Solidus 47.0 °C
117 °F
Liquidus 47.0 °C
117 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 44.7 %
44.7 %
Cadmium, Cd 5.3 %
5.3 %
Indium, In 19.1 %
19.1 %
Lead, Pb 22.6 %
22.6 %
Tin, Sn 8.3 %
8.3 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000380 ohm-cm
0.0000380 ohm-cm