Thermal Properties Metric English Comments
Solidus 545.0 °C
1013 °F
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..